Project Description

Surface:                 Steel cover of hardening furnaces

Purpose:                Prevent heat radiation and save energy

 

Coating Solution

 

Initially furnace was cleaned to remove grease and dirt. Then HOT SURFACE COATING was applied in 2 layers (total thickness = 3mm). When dry, surface was sealed with a silver grey color paint.

 

Results

 

 

Initial surface temperature on the doors: 100°C

After 3mm HSC: 65°C - Reduced surface temperature by 35%

 

Initial surface temperature on the rest of the furnace: 65°C

After 3mm HSC: 45°C - Reduced surface temperature by 31%